Almost every DTF problem comes from heat, pressure or timing. Find your symptom below.

Transfer not sticking or edges lifting

Cause: light pressure or a skipped pre-press. The center bonds but the perimeter does not.
Fix: increase to firm pressure, pre-press the garment for 5 seconds, and add a 7 second second press under parchment.

Cracking after the first wash

Cause: temperature too low or first press too short.
Fix: check the platen with an infrared thermometer. If the display says 305 F but the platen is 290 F, calibrate the press or extend the press time to 15 to 16 seconds.

Print lifts with the film

Cause: peeling too hot on a cold-peel film, or waiting too long on a warm-peel film.
Fix: identify your film type. If art lifts with the film, lay it back down and re-press for 5 seconds before peeling again. See cold peel vs warm peel.

White edges around the design

Cause: excess white ink at the film edge, not an application issue.
Fix: trim extra white with sharp scissors before pressing, or send us a photo and we will check the reprint.

Cloudy or hazy finish

Cause: used parchment or moisture.
Fix: use a fresh sheet of parchment for each few presses and keep humidity in check in the press area.

Sticky or rubbery feel

Cause: skipped second press.
Fix: second press for 5 to 7 seconds under parchment or a Teflon sheet.

Bubbling

Cause: moisture in the garment.
Fix: pre-press for 5 seconds before you place the transfer.

Seams and pockets

Use a pressing pillow so the area under the print is flat and gets full pressure.

Still stuck?

Send us a photo and your press settings. Check the settings by fabric first, then contact us.

Frequently asked questions

Why is my DTF transfer not sticking?

The usual causes are light pressure, low platen temperature or a skipped pre-press. Raise pressure, verify temperature with a thermometer and pre-press for 5 seconds.

Why is my DTF print cracking?

Cracking after a wash is usually under-heating or too little press time. Verify the platen temperature and extend the press time slightly.

Can I re-press a transfer that did not stick?

Yes. Cover it and re-press for about 5 seconds, then peel again.

Latino-Owned Business | We Speak English & EspañolSe habla español.
New
Blog DTF vs Screen Printing: Cost Per Shirt Blog DTF Transfers for Schools, Teams and Clubs Blog DTF Transfer Troubleshooting Blog DTF Heat Press Settings by Fabric Blog DTF Gang Sheet Layout Guide Blog DTF File Prep Checklist Blog Cold Peel vs Warm Peel DTF New page Transferencias DTF en Dallas, Texas New page DTF Transfers in Sunnyvale, TX New page DTF Transfers in Seagoville, TX
$

Request a free sample pack

We'll ship sample materials so you can feel before you buy. No purchase necessary.

Which samples? (pick all that apply)

One pack per household per 30 days. US addresses only. Allow 5-7 business days for delivery.

New Get Early Access